Polymer Property : Tensile Strength = 15790 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 108.9 MPa
15790 psi
ASTM D638
E-Polymers SEPAZ® N1140 Nanoclay 4% Medium Viscosity Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..