Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 10.69 MPa | >= 1551 psi | ASTM D412 Method A |
Seals Eastern 7042U Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |