Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 11.0 - 15.0 MPa | 1600 - 2180 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Tensile Strength | 11.0 - 15.0 MPa | 1600 - 2180 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Tensile Strength | 11.0 - 15.0 MPa | 1600 - 2180 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Tensile Strength | 11.0 - 15.0 MPa | 1600 - 2180 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |