Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 10.2 MPa | 1480 psi | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-70A/B Elastomer KEG2000-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum.. |
|||
Tensile Strength | 10.20 MPa | 1480 psi | ASTM D412 |
E-Polymers EFLEX® S1030 General S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas.. |