Polymer Property : Tensile Strength = 145000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 1000 MPa
145000 psi
20% Reduction of Section
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar
Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan..
Tensile Strength 1000 - 1140 MPa

@Thickness <=25.4 mm
145000 - 165000 psi

@Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Tensile Strength >= 1000 MPa

@Treatment Temp. 579.4 °C,
Time 14400 sec
>= 145000 psi

@Treatment Temp. 1075 °F,
Time 4.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..