Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1400 - 1460 MPa | 203000 - 212000 psi | |
Plansee DENAL® 920 159 20 Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |
|||
Tensile Strength | 1400 MPa | 203000 psi | 44 HRC |
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |