Tensile Strength 14.24 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2065 psi

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
S&E Specialty Polymers GA-509OR PVC
Application: FR, UV and oil resistant PVC based compound with good low temperature properties.Information provided by S&E Specialty Polymers