Polymer Property : Tensile Strength = 13517 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 93.195 MPa
13517 psi
ASTM D638
E-Polymers TEKAMID® HG10L 10% Glass Fiber Reinforced High Impact PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
Tensile Strength 93.195 MPa
13517 psi
ASTM D638
E-Polymers SEPAZ® LC30 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..