Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.10 MPa | 1320 psi | |
Momentive Performance Materials TSE 221-5U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.10 MPa | 1320 psi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6156 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |