Polymer Property : Tensile Strength = 132.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 132.4 MPa
19210 psi
ASTM D638
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Tensile Strength 132.4 MPa
19210 psi
ASTM D638
E-Polymers SEPAZ® C130GP 30% Glass Fiber Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..