Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.0252 MPa | 1309.0 psi | ASTM D412 |
E-Polymers EFLEX® V2080 SEBS/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |