Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 13.248 MPa @Temperature 100 °C, Time 346000 sec |
1921.5 psi @Temperature 212 °F, Time 96.0 hour |
Oil Aged |
S&E Specialty Polymers TufFlex™ GTPE-2272SG-K8 TPE Compound Application: A flame retardant, matte finish, 90°C oil resistant, flexible TPE jacketing material.Information provided by S&E Specialty Polymers |