Polymer Property : Tensile Strength = 13.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.00 - 13.0 MPa
1160 - 1890 psi
molded; ASTM D4745
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..