Mechanical Properties Metric English Comments
Tensile Strength 8.85 MPa

@Treatment Temp. 140 °C,
Time 3.629e+6 sec
1280 psi

@Treatment Temp. 284 °F,
Time 1008 hour
heat aging; ASTM D573-99
Multibase TPSiV® 3111-70A Thermoplastic Elastomer
TPSiV™ material for injection molding and extrusion applicationsAPPLICATIONS: Solution for appliance, sports and leisure, and construction applications where excellent hydrolysis resistance, high a..
Tensile Strength 8.80 MPa
1280 psi
ISO 37
Multibase TPSiV® 4000-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Tensile Strength 8.83 MPa

@Strain 100 %
1280 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B8501 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible Vinyl compound for hose and tubing applications with enhanced physical characteristics.Information provided by PolyOne
Tensile Strength >= 8.83 MPa
>= 1280 psi
ASTM D 638
Karina E CAK 75-48/1 Black PVC Compound
Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 8.83 MPa
>= 1280 psi
ASTM D 638
Karina 653D10/1-C-IS White PVC Compound
Anti fungus PVC compound for extrusion/drain blow molding.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 8.83 MPa
>= 1280 psi
ASTM D 638
Karina 75/200 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 8.83 MPa
>= 1280 psi
ASTM D 638
Karina 75/202 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 8.83 MPa
>= 1280 psi
ASTM D 638
Karina CAK 75-48/1 Black PVC Compound
Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 8.83 MPa
>= 1280 psi
ASTM D 638
Karina 760-48/1-E-AC-LF Black PVC Compound
Flame retardant and lead and cadmium free PVC compound recommended for extrusion and injection of parts for general purposes.Information provided by Karina Indústria e Comércio de Plásticos..
Tensile Strength 8.80 MPa
1280 psi
Shin-Etsu Silicones LIMSâ„¢ KE1950-30A/B Elastomer
KE-1950-30 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy ..