Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.69 MPa | 1260 psi | ASTM D412 |
S&E Specialty Polymers TufLite™ GTPE-2001T TPE Application: A Thermoplastic Elastomer (TPE) designed for injection molding applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 8.69 MPa | 1260 psi | Silicone Compound Property; Arlon SQA-TMS-009 |
Arlon 910-10Rxx-P1 0.010" Cured, Self-Fusing Silicone Rubber 1.0 inch wide, 0.010" thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Tensile Strength | 8.69 MPa | 1260 psi | Silicone Property; Arlon SQA-TMS-009 |
Arlon 930-10Rxx-P1 0.030" Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |