Tensile Strength 8.088 MPa
1173 psi
Silicone Property; ASTM D412
Arlon R38726R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeThis data represents typical values for the production material. The..
Tensile Strength 8.088 MPa
1173 psi
Silicone Property; ASTM D412
Arlon R38726R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeProduct Use: Flexible heater substrateAppearance: Red colored, high ..