Mechanical Properties Metric English Comments
Tensile Strength 800 MPa
116000 psi
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..