Polymer Property : Tensile Strength = 107.91 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 107.91 MPa
15651 psi
ASTM D638
E-Polymers TEKAFIN® PH50G3 30% Glass Fiber Reinforced High Strength Compounded-PP
Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I..
Tensile Strength 107.91 MPa
15651 psi
ASTM D638
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy
PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan..