Polymer Property : Tensile Strength = 107 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 0.740 MPa
107 psi
ISO 7214 1998
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 8225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9035 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9335 MG 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9435 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to..
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..