Mechanical Properties Metric English Comments
Tensile Strength 7.026 MPa
1019 psi
Silicone Property; ASTM D412
Arlon LW50125R##-P1 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll lengt..