Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.80 MPa | 261 psi | ISO 37 |
Premix Thermoplastics PRETHERM TPE 1075 Thermoplastic Elastomer, Boron Nitride / SEBS compound PRETHERM TPE 1075 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It can be used as gap filler between processor and heat sink or co-.. |
|||
Tensile Strength | >= 1.80 MPa | >= 261 psi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Tensile Strength | 1.80 MPa | 261 psi | ISO 37 |
AlphaGary Evoprene™ GC 5677 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |