Polymer Property : Tensile Strength = 0.586 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 0.586 MPa
85.0 psi
ASTM D412
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer
This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist..