Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.483 MPa | 70.0 psi | Typical; ASTM D3574-75 Test E |
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Tensile Strength | 0.483 MPa | 70.0 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ P292HD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Tensile Strength | 0.483 MPa | 70.0 psi | |
Monmouth Rubber & Plastics Durafoam™ P291HD EPDM Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ i.. |