Mechanical Properties Metric English Comments
Tensile Strength 0.414 MPa
60.0 psi
Typical; ASTM D3574-75 Test E
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
Tensile Strength >= 0.414 MPa
>= 60.0 psi
ASTM D3574-75 Test E
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade
Thickness: 0.125"- 0.500"Color: BlackInformation provided by Rogers Corporation.
Tensile Strength 0.414 MPa
60.0 psi
Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam
This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load b..