Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.320 MPa | 46.4 psi | ISO 7214 1998 |
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Tensile Strength | 0.320 MPa | 46.4 psi | ASTM D 412 |
Eurofoam Porocell POR 304 CM-S EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.320 MPa | 46.4 psi | ASTM D 412 |
Eurofoam Porocell 251 BG NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |