Polymer Property : Tensile Strength = 0.100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 0.100 MPa
14.5 psi
ASTM D 412
Eurofoam Porocell POR 304 CM-OPC EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Tensile Strength 0.100 MPa
14.5 psi
ASTM D 412
Eurofoam Porocell POR 304 B-OPC EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.