Mechanical Properties Metric English Comments
Tear Strength, Total 2540 N
571 lb (f)
MD, Graves; ASTM D1004
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..