Mechanical Properties Metric English Comments
Tear Strength, Total 93.0 N
20.9 lb (f)
M.D., PPT; ASTM D2582
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Tear Strength, Total 93.0 N
20.9 lb (f)
T.D., PPT; ASTM D2582
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Tear Strength, Total 93.0 N
20.9 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..