Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 63.6 N | 14.3 lb (f) | Initial in TD; ASTM D1004 |
DuPont™ Nomex® N196 Paper, 15 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |