Polymer Property : Tear Strength, Total = 12.4 lb (f) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 55.0 N
12.4 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Tear Strength, Total 55.0 N
12.4 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
Tear Strength, Total 55.0 N
12.4 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..