Mechanical Properties Metric English Comments
Tear Strength, Total 45.0 N
10.1 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..