Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Impact = 90.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 3743 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 6557 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 1080 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 112 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 117 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 6543 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 1543 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..