Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 66.7 J/cm | 125 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 4522 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 66.7 J/cm | 125 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 4522 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 66.7 J/cm | 125 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 7579 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |