Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 328 J/cm | 615 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 7562 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |