Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 339 J/cm | 635 ft-lb/in | Filling |
Hexcel® HexForce™ 5353 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |