Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 294 J/cm | 550 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 332 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 294 J/cm | 550 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 3434 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 294 J/cm | 550 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 3434 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 294 J/cm | 550 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 6781 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 294 J/cm | 550 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 232 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 294 J/cm | 550 ft-lb/in | Warp |
Hexcel® HexForce™ 372 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Tensile Impact | 294 J/cm | 550 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1582 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |