Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 260 J/cm | 487 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co. |