Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 854 J/cm | 1600 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 3788 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |