Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 112 J/cm | 210 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1692 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 112 J/cm | 210 ft-lb/in | Warp |
Hexcel® HexForce™ 345 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Tensile Impact | 112 J/cm | 210 ft-lb/in | Filling |
Hexcel® HexForce™ 345 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Tensile Impact | 112 J/cm | 210 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1165 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |