Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 55 µm/km | 55 µm/km | |
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data) This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap.. |