Mechanical Properties Metric English Comments
K Factor (ISO) 18 µm/km
18 µm/km
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, ..