Magnetic Properties | Metric | English | Comments |
---|---|---|---|
Core Loss | <= 65.0 W/kg @Frequency 700 Hz |
<= 29.5 W/lb @Frequency 700 Hz |
at 1T, Indicative |
ArcelorMittal Speed 35-510 Electrical Steel Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |