Magnetic Properties | Metric | English | Comments |
---|---|---|---|
Core Loss | 0.00362 W/kg @Magnetic Field 0.100 T, Frequency 50.0 Hz |
0.00164 W/lb @Magnetic Field 0.100 T, Frequency 50.0 Hz |
ASTM A804, 0.27 mm |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Core Loss | 0.00361 W/kg @Magnetic Field 0.100 T, Frequency 50.0 Hz |
0.00164 W/lb @Magnetic Field 0.100 T, Frequency 50.0 Hz |
ASTM A804, 0.30 mm |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |