Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Pressure | 44.583 bar | 33440 torr | |
Shandong Dongyue Shenzhou New Material Co Vinylidene Fluoride (VDF) Conformable with: Q/DYS 007-2007VDF is a kind of colorless gas under normal temperature and pressure, nontoxic, flammable, with little ether odor. It has the common gender of alkene, and can be pol.. |