Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Pressure | 40.0 bar | 30000 torr | |
Solvay Chemicals 1,2,3-Trichloropropane Colourless liquid, mainly used as chemical intermediate.EINECS Number: 202-486-1/CAS Number: 96-18-4/UN number: 2810Information provided by Solvay |