Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Pressure | 37.9 bar | 28400 torr | |
Solvay Specialty Polymers Meforex® 143a Ozone-Friendly CFC Replacement Formula: CH3CF3; Name: 1,1,1 Trifluoroethane. Replaces R 502. Refrigerant blends components for low and middle temperatures.Information provided by Solvay Solexis, Inc. |