Acetaldehyde 0.600 ppm
0.600 ppm
Target; M2E-75-007
Indorama Ventures Mexico Polyclearâ„¢ Splash 3301 PET Resin
Description: La resina Polyclear® Splash PET 3301 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.74 dl/g. La resina Polyclear® Splash PET 3301 ha sido ..