Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) 30 ppm
30 ppm
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive
TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi..