Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) 875 ppm
875 ppm
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT
ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a..