Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Na (Sodium) | 22 ppm | 22 ppm | |
Epoxy Technology EPO-TEK® E3037 Epoxy Material Description: A single component, electrically conductive, thixotropic silver-filled epoxy for die-attach and SMD-attach inside hybrid microelectronics.Information Provided by Epoxy Technolo.. |